產品展示
【簡單介紹】
【詳細說明】
性能項目 | 試驗條件[狀態] | 測試方法 | 測試數據 | 數據單位 | |||||||||||||
基本性能 | 吸水率 | 24小時,73?H | ASTM D-570 | 0.250 | % | ||||||||||||
吸水率 | 平衡,73?H | ASTM D-570 | 1.25 | % | |||||||||||||
熔體流動速率 | --- | ASTM D-1238 | 8.9 | g/10min | |||||||||||||
物理性能 | 模具收縮率 | --- | ASTM D-955 | 5-7 | in/inE-3 | ||||||||||||
固體比重 | --- | ASTM D-792 | 1.27 | --- | |||||||||||||
機械性能 | IZOD缺口沖擊強度 | --- | ASTM D-256 | 1.0 | ft-lb/in | ||||||||||||
屈服抗拉強度 | --- | ASTM D-638 | 15200 | Psi | |||||||||||||
屈服抗拉伸長 | --- | ASTM D-638 | 7.0 | % | |||||||||||||
斷裂抗拉伸伸長 | --- | ASTM D-638 | 60.0 | % | |||||||||||||
屈服撓曲強度 | --- | ASTM D-790 | 22000 | Psi | |||||||||||||
撓曲模量 | --- | ASTM D-790 | 480000 | Psi | |||||||||||||
洛氏硬度 | --- | ASTM D-785 | 109 | Psi | |||||||||||||
泰伯磨耗量 | --- | ASTM D-1044 | 10 | mg/1000次 | |||||||||||||
IZOD無缺口沖擊強度 | --- | ASTM D-4812 | 25.0 | ft-lb/in | |||||||||||||
電氣性能 | 體積電阻率 | --- | ASTM D-257 | 1×1017 | Ω.cm | ||||||||||||
介電強度 | 62mils | ASTM D-149 | 831 | V/mil | |||||||||||||
介電常數 | 1KHz | ASTM D-150 | 3.15 | --- | |||||||||||||
損耗因數 | 1KHz | ASTM D-150 | 0.0012 | --- | |||||||||||||
熱 性 能 | 燃燒性 | --- | UL 94 | 5VA | class | ||||||||||||
維卡軟化點 | --- | ASTM D-1525 | 426 | ?H | |||||||||||||
熱變形溫度 | 66Psi | ASTM D-648 | 410 | ?H | |||||||||||||
熱變形溫度 | 264Psi | ASTM D-648 | 392 | ?H | |||||||||||||
| --- |
|
|
| |||||||||||||
| --- |
|
|
|
相關產品
- POM GH-25 日本寶理
- TPE 7246 美國杜邦
- K膠 KR-03 菲利浦
- MS TX-100S 日本電氣化學
- AS PN-117 中國臺灣奇美
- LCP 6130L 美國杜邦
- LCP E130i 日本寶理
- PPS E604 日本東麗
- PPS 1140A6 日本寶理
- PBT 310SE0 美國GE
- PBT 420SE0 美國GE
- PBT 357 美國GE
- PEI 1000 美國GE
- PET FR530 美國杜邦
- TPU 6386A 德國拜耳
- TPU 285 德國拜耳
- PPO PX1005X 美國GE
- TPX MX002 日本三井
- TPX MX004 日本三井
- TPX RT18 日本三井
- PC/ABS T65 德國拜耳
- PC/ABS C1200HF 美國GE
- PC/ABS C2950 美國GE
- PA66 1300G 日本旭化成
- PA66 1300S 日本旭化成
- PA66 ST801 美國杜邦
- PA66 101L 美國杜邦
- PA6 1013B 日本宇部
- PMMA 560F 日本旭化成
- PC 2405 德國拜耳
- PC 6555 德國拜耳
- PC L-1250Y 日本帝人
- POM 100P 美國杜邦