Hostaform S 9364 XAP POM Ticona
Hostaform S 9364 XAP POM Ticona
Hostaform TF-10XAP POM Ticona
Latan 13 G/30 POM LATI
Latan 13 S/30 POM LATI
Latan 13 G/30 POM LATI
Hostaform S 9364 XAP POM Ticona材料物性表如下:
Physical | Nominal Value | Unit | Test Method |
Density | 1.37 | g/cm3 | ISO 1183 |
Melt Volume-Flow Rate (MVR) (190°C/2.16 kg) | 0.244 | in3/10min | ASTM D1238 |
Molding Shrinkage | ISO 294-4 | ||
Across Flow | 1.5 | % | |
Flow | 1.6 | % | |
Water Absorption (Saturation, 73°F) | 0.80 | % | ISO 62 |
Mechanical | Nominal Value | Unit | Test Method |
Tensile Modulus | 239000 | psi | ISO 527-2/1A/1 |
Tensile Stress (Yield) | 6240 | psi | ISO 527-2/1A/50 |
Tensile Strain (Yield) | 16 | % | ISO 527-2/1A/50 |
Flexural Modulus (73°F) | 225000 | psi | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
Charpy Notched Impact Strength | ISO 179/1eA | ||
-22°F | 5.2 | ft·lb/in2 | |
73°F | 10 | ft·lb/in2 | |
Charpy Unnotched Impact Strength | ISO 179/1eU | ||
-22°F | No Break | ||
73°F | No Break |
Thermal | Nominal Value | Unit | Test Method |
Heat Deflection Temperature | |||
66 psi, Unannealed | 284 | °F | ISO 75-2/B |
264 psi, Unannealed | 167 | °F | ISO 75-2/A |
Melting Temperature 2 | 331 | °F | ISO 11357-3 |
CLTE | ISO 11359-2 | ||
Flow | 0.000067 | in/in/°F | |
Transverse | 0.000061 | in/in/°F |
Celcon WR25Z POM Ticona
Celcon WR25Z POM Ticona
Celcon WR90Z POM Ticona
Hostaform AM90S Plus POM Ticona
:鄧
:86-
傳真號碼:86-
地址:中國 廣東 東莞 東莞市 樟木頭鎮 塑膠原料市場
Hostaform S 9364 XAP POM Ticona靈活性其它產品
Hostaform S 9364 XAP POM Ticona靈活性
Hostaform S 9363 POM Ticona抗沖擊性
Hostaform S 9243 POM Ticona耐化學性
Hostaform S 27072 WS 10/1570 POM Ticona
Hostaform S 27064 POM Ticona超高韌性
Hostaform MT8F01 POM Ticona醫療應用
Hostaform MT24U01 POM Ticona泰科納
Hostaform MR130ACS POM Ticona泰科納
Hostaform LX90GC15 POM Ticona玻纖15%
Hostaform LX90 POM Ticona泰科納