優(yōu)勢(shì)說(shuō)明:PA66吸水量:每1%吸水量體積增加0.003in,在50%的相對(duì)濕度,23℃的氣溫吸水量是2.5%。收縮率為2.25%,比重1.14G/CM3詳細(xì)說(shuō)明:
1.PA66吸水量:每1%吸水量體積增加0.003in,在50%的相對(duì)濕度,23℃的氣溫吸水量是2.5%。收縮率為2.25%,比重1.14G/CM3
: 本公司可以免費(fèi)提供各種材料認(rèn)
證
產(chǎn)品說(shuō)明 | |
Vydyne® R513H BK Nylon resins are general purpose polyamide, 13% glass fiber reinforced, and heat stabilized resins. Available in natural and black. Ascend Performance Materials has engineering data available for this resin, including 50% RH data. Please contact your customer service representative. They are injection molding grade resins that are lubricated for machine feed, flow and mold release. Vydyne R513H is a member of a glass reinforced family supplied by Ascend Performance Materials which also includes 33% and 43% glass fiber loadings. These resins provide a range of cost performance products in which tensile strength is increased with the increasing glass fiber loadings. Glass reinforced Vydyne resins provide a higher heat distortion temperature, better resistance to creep, higher impact and better dimensional stability when compared with unreinforced Nylon 6,6. These products have good chemical resistance to a broad range of chemicals including many aliphatic and aromatic hydrocarbons found in most solvents, gasoline, hydraulic fluids, greases and machine oils. Vydyne R513H Series resins have tensile strength and modulus properties just below aluminum and zinc and can replace these metals in numerous applications due to an excellent balance of properties. Reduction in production costs, energy consumption, and part weight are key advantages of Vydyne glass reinforced Nylon 6,6 resins over aluminum and/or zinc die cast parts. Vydyne R513H Series are heat stabilized and formulated to minimize the oxidative and thermal degradation of the nylon polymer when exposed to elevated temperatures for extended periods of time. Vydyne R513H provides improved retention of physical properties under exposure to long-term heat. The continuous operating use temperature is 275°F and short-term peak temperatures as high as 475°F. Typical Applications/End Uses: Vydyne R513H Series resins have been used for many under-the-hood automotive applications, motor housings for power tools, and garden appliances. These resins have also been used in miscellaneous brackets, gears, and clips, which require high rigidity and strength. | |
總體 | |
材料狀態(tài) | 已商用:當(dāng)前有效 |
資料 1 | Processing (English)Technical Datasheet (English) |
UL 黃卡 2 | E70062-249082 |
搜索 UL 黃卡 | Ascend Performance Materials LLC.Vydyne® |
供貨地區(qū) | 北美洲歐洲亞太地區(qū) |
填料/增強(qiáng)材料 | 玻璃纖維增強(qiáng)材料, 13% 填料按重量 |
添加劑 | 熱穩(wěn)定劑潤(rùn)滑劑 |
性能特點(diǎn) | 剛性,高高強(qiáng)度經(jīng)潤(rùn)滑抗溶解性良好的流動(dòng)性耐化學(xué)性良好耐汽油性耐油性能耐油脂性能熱穩(wěn)定性脫模性能良好 |
用途 | 齒輪動(dòng)力/其它工具汽車(chē)的發(fā)動(dòng)機(jī)罩下的零件型號(hào) |
機(jī)構(gòu)評(píng)級(jí) | ASTM D 4066 PA012G15ASTM D 6779 PA012G15FED L-P-410AMIL M-20693B |
UL 檔案號(hào) | E70062 |
外觀 | 黑色自然色 |
形式 | 顆粒料 |
加工方法 | 注射成型 |
多點(diǎn)數(shù)據(jù) | Isothermal Stress vs. Strain (ISO 11403-1) |
物理性能 | 干燥 | 調(diào)節(jié)后的 | 單位制 | 測(cè)試方法 |
密度 | 1.22 | -- | g/cm3 | ISO 1183 |
收縮率 | ISO 294-4 | |||
橫向流量: 73°F, 0.0787 in | 1.0 | -- | % | |
流量: 73°F, 0.0787 in | 0.50 | -- | % | |
吸水率 | ISO 62 | |||
73°F, 24 hr | 1.0 | -- | % | |
平衡, 73°F, 50% RH | 2.2 | -- | % |
機(jī)械性能 | 干燥 | 調(diào)節(jié)后的 | 單位制 | 測(cè)試方法 |
拉伸模量 (73°F) | 899000 | 566000 | psi | ISO 527-2 |
拉伸應(yīng)力 (斷裂, 73°F) | 17700 | 10900 | psi | ISO 527-2 |
拉伸應(yīng)變 (斷裂, 73°F) | 3.0 | 13 | % | ISO 527-2 |
彎曲模量 (73°F) | 754000 | 457000 | psi | ISO 178 |
彎曲強(qiáng)度 (73°F) | 29000 | 15400 | psi | ISO 178 |
泊松比 | 0.41 | -- | ISO 527-2 | |
沖擊性能 | 干燥 | 調(diào)節(jié)后的 | 單位制 | 測(cè)試方法 |
簡(jiǎn)支梁缺口沖擊強(qiáng)度 | ISO 179 | |||
-22°F | 3.8 | -- | ft·lb/in2 | |
73°F | 3.8 | -- | ft·lb/in2 | |
簡(jiǎn)支梁缺口沖擊強(qiáng)度 | ISO 179 | |||
-22°F | 17 | -- | ft·lb/in2 | |
73°F | 18 | -- | ft·lb/in2 | |
懸壁梁缺口沖擊強(qiáng)度 (73°F) | 2.4 | -- | ft·lb/in2 | ISO 180 |
熱性能 | 干燥 | 調(diào)節(jié)后的 | 單位制 | 測(cè)試方法 |
熱變形溫度 | ||||
66 psi, 未退火 | 496 | -- | °F | ISO 75-2/B |
264 psi, 未退火 | 464 | -- | °F | ISO 75-2/A |
維卡軟化溫度 | 482 | -- | °F | ISO 306/B |
溶融溫度(DSC) | 500 | -- | °F | ISO 3146 |
線形膨脹系數(shù) | ISO 11359-2 | |||
流動(dòng): 73 到 131°F, 0.0787 in | 2.2E-6 | -- | in/in/°F | |
橫向: 73 到 131°F, 0.0787 in | 6.1E-6 | -- | in/in/°F | |
RTI Elec | UL 746 | |||
0.0280 in | 284 | -- | °F | |
0.0591 in | 284 | -- | °F | |
0.118 in | 284 | -- | °F | |
RTI Imp | UL 746 | |||
0.0280 in | 248 | -- | °F | |
0.0591 in | 248 | -- | °F | |
0.118 in | 248 | -- | °F | |
RTI Str | UL 746 | |||
0.0280 in | 257 | -- | °F | |
0.0591 in | 284 | -- | °F | |
0.118 in | 284 | -- | °F |
電氣性能 | 干燥 | 調(diào)節(jié)后的 | 單位制 | 測(cè)試方法 |
體積電阻率 (0.118 in) | 4.0E+15 | -- | ohm·cm | IEC 60093 |
耐電強(qiáng)度 3 (73°F, 0.118 in) | 380 | -- | V/mil | IEC 60243-1 |
耐電弧性 (0.118 in) | PLC 6 | -- | ASTM D495 | |
相比耐漏電起痕指數(shù)(CTI) (0.118 in) | PLC 2 | -- | UL 746 | |
漏電起痕指數(shù) (0.118 in) | 250 到 400 | -- | V | IEC 60112 |
高電弧燃燒指數(shù)(HAI) | UL 746 | |||
0.0280 in | PLC 0 | -- | ||
0.0591 in | PLC 0 | -- | ||
0.118 in | PLC 0 | -- | ||
高電壓電弧起痕速率 (HVTR) (0.118 in) | PLC 1 | -- | UL 746 | |
熱絲引燃 (HWI) | UL 746 | |||
0.0280 in | PLC 4 | -- | ||
0.0591 in | PLC 3 | -- | ||
0.118 in | PLC 4 | -- | ||
可燃性 | 干燥 | 調(diào)節(jié)后的 | 單位制 | 測(cè)試方法 |
UL 阻燃等級(jí) | UL 94 | |||
0.0280 in, All colors | HB | -- | ||
0.0591 in, All colors | HB | -- | ||
0.118 in, All colors | HB | -- | ||
灼熱絲易燃指數(shù) | IEC 60695-2-12 | |||
0.0280 in | 1250 | -- | °F | |
0.0591 in | 1250 | -- | °F | |
0.118 in | 1250 | -- | °F | |
熱燈絲點(diǎn)火溫度 | IEC 60695-2-13 | |||
0.0280 in | 1290 | -- | °F | |
0.0591 in | 1290 | -- | °F | |
0.118 in | 1290 | -- | °F | |
極限氧指數(shù) | 25 | -- | % | ASTM D2863 |
注射 | 干燥 | 單位制 | |
干燥溫度 | < 158 | °F | |
干燥時(shí)間 | 1.0 到 3.0 | hr | |
建議注入量 | 40 到 80 | % | |
建議的zui大回制料比例 | 25 | % | |
螺筒后部溫度 | 536 到 590 | °F | |
螺筒中部溫度 | 536 到 590 | °F | |
螺筒前部溫度 | 536 到 590 | °F | |
射嘴溫度 | 536 到 590 | °F | |
加工(熔體)溫度 | 545 到 581 | °F | |
模具溫度 | 149 到 203 | °F | |
注塑溫度 | 7980 到 20300 | psi | |
注射速度 | 快速 | ||
保壓 | 7980 到 20300 | psi | |
背壓 | 29.0 到 145 | psi | |
螺桿轉(zhuǎn)速 | 60 到 120 | rpm | |
合模力 | 1.9 到 4.5 | tons/in2 | |
墊層 | 0.118 到 0.252 | in | |
注射說(shuō)明 | |||
Injection Time: <1 to 2.5 sec |
:何生
:86-
傳真號(hào)碼:86-
地址:廣東 東莞市
PA66美國(guó)首諾 R513H BK良好的流動(dòng)性 耐化學(xué)性良好 耐汽油性其它產(chǎn)品
PA66美國(guó)首諾 R513H BK良好的流動(dòng)性 耐化學(xué)性良好 耐汽油性
PA66美國(guó)首諾 R513H BK玻璃纖維增強(qiáng)材料, 13% 填料按重量
PA66美國(guó)首諾 R-220 礦物填料, 40% 填料按重量
PA66美國(guó)首諾 R-220齒輪 動(dòng)力/其它工具
PA66美國(guó)首諾 R-220剛性,汽車(chē)外部零件 凸輪
PA66美國(guó)首諾 R-220剛性,高 抗溶解性 抗撞擊性,良好 良好的強(qiáng)
PA66美國(guó)首諾 R-220熱穩(wěn)定性 韌性良好 延展性
PA66美國(guó)首諾 R-220耐化學(xué)性良好 耐汽油性 耐熱性,高 耐油性能
PA66美國(guó)首諾 R350-GF25 玻璃纖維增強(qiáng)材料, 25%
PA66美國(guó)首諾 J350-GK30 玻璃珠, 30% 填料按重量